logo
Dom ProduktyMagnez żelazokrzemowy

Magnesium Ferrosilicon 5% 6% 7% for Spheroidizing Treatment and Nodular Cast Iron Production

Im Online Czat teraz

Magnesium Ferrosilicon 5% 6% 7% for Spheroidizing Treatment and Nodular Cast Iron Production

Magnesium Ferrosilicon 5% 6% 7% for Spheroidizing Treatment and Nodular Cast Iron Production
Magnesium Ferrosilicon 5% 6% 7% for Spheroidizing Treatment and Nodular Cast Iron Production Magnesium Ferrosilicon 5% 6% 7% for Spheroidizing Treatment and Nodular Cast Iron Production Magnesium Ferrosilicon 5% 6% 7% for Spheroidizing Treatment and Nodular Cast Iron Production Magnesium Ferrosilicon 5% 6% 7% for Spheroidizing Treatment and Nodular Cast Iron Production Magnesium Ferrosilicon 5% 6% 7% for Spheroidizing Treatment and Nodular Cast Iron Production

Duży Obraz :  Magnesium Ferrosilicon 5% 6% 7% for Spheroidizing Treatment and Nodular Cast Iron Production

Szczegóły Produktu:
Miejsce pochodzenia: Chiny
Nazwa handlowa: ZHENAN
Orzecznictwo: ISO9001:2015
Numer modelu: FeSiMg 3-8
Zapłata:
Minimalne zamówienie: Zbywalny
Cena: Zbywalny
Szczegóły pakowania: Big Bag 1MT lub na życzenie klienta
Czas dostawy: 7-10 dni roboczych po otrzymaniu płatności
Zasady płatności: Akredytywa, T/T, Western Union
Możliwość Supply: 2000MT/miesiąc

Magnesium Ferrosilicon 5% 6% 7% for Spheroidizing Treatment and Nodular Cast Iron Production

Opis
Tworzywo: żelazokrzem magnez Kolor: Szary
Kompozycja chemiczna: Si Fe Al SP Kształt: bryła
Uszczelka: W Big Bagach 1MT Aplikacja: Produkcja stali
Podkreślić:

Magnesium Ferrosilicon 5% spheroidizing

,

Magnesium Ferrosilicon 6% nodular cast iron

,

Magnesium Ferrosilicon 7% production

Why Spheroidizing Treatment Depends on Magnesium Ferrosilicon 5% 6% 7% Spheroidizing treatment is a controlled reaction, and the alloy is the control. Magnesium ferrosilicon 5% 6% 7% gives the treatment station three settings: a low-magnesium alloy for short, cool pours, a middle alloy for general work, and a high-magnesium alloy for sections that stay liquid long after the ladle is empty. Choose too low and the last metal poured comes out with flake graphite; choose too high

Szczegóły kontaktu
Zhenan Metallurgy Co., Ltd

Osoba kontaktowa: Mr. xie

Wyślij zapytanie bezpośrednio do nas (0 / 3000)